Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® T7300EG10 LS BK23346 - PA*-GF50 - BASF

Material Data Center offers the following functions for Ultramid® T7300EG10 LS BK23346:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid T datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Glass-fiber reinforced, heat aging resistant injection molding grade with excellent surface quality based on semi-crystalline polyamides with partially aromatic content. The product can be characterized as compound with very high strength and stiffness even after moisture uptake.

Markets & applications
Automotive: structural parts, metal replacement, brake parts, interior, powertrain
E&E: electrical appliances, cell phones
Consumer goods: home appliances, consumer electronics, furniture fittings
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 7 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
Contração após a moldagem, paralelo 0.5 / * % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.7 / * % ISO 294-4, 2577
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 17700 / 16600 MPa ISO 527
Tensão na ruptura 255 / 210 MPa ISO 527
Deformação na ruptura 2.8 / 3 % ISO 527
Resistência ao impacto Charpy , +23°C 108 / 100 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 90 / 88 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 15 / 15 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 14 / 14 kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 255 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 240 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 255 / * °C ISO 75-1/-2
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Absorção de umidade 1.2 / * % Sim. to ISO 62
Densidade 1600 / - kg/m³ ISO 1183
Propriedades específicas do materialSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de viscosidade 134 / * cm³/g ISO 307, 1157, 1628
Produção de amostra para testeValorUnidadeMétodo de ensaio
ISO Dados
Moldagem por injeção, temperatura da massa 310 °C ISO 294
Moldagem por injeção, temperatura do molde 100 °C ISO 294
Moldagem por injeção, velocidade de injeção 200 mm/s ISO 294
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 110 °C -
Pré-secagem - tempo 8 h -
Umidade do processamento ≤0.15 % -
Temperatura da massa 300 - 320 °C -
Temperatura do molde 80 - 120 °C -
Tempo de residência máximo 5 min -
Diagrama
Viscosidade - taxa de cisalhamento , Ultramid® T7300EG10 LS BK23346, PA*-GF50, BASF
Tensão de cisalhamento - taxa de cisalhamento , Ultramid® T7300EG10 LS BK23346, PA*-GF50, BASF
Tensão - deformação , Ultramid® T7300EG10 LS BK23346 (dry), PA*-GF50, BASF
Tensão - deformação , Ultramid® T7300EG10 LS BK23346 (cond.), PA*-GF50, BASF
Módulo secante - deformação , Ultramid® T7300EG10 LS BK23346 (dry), PA*-GF50, BASF
Módulo secante - deformação , Ultramid® T7300EG10 LS BK23346 (cond.), PA*-GF50, BASF
Tensão - deformação (isocrônico) 23°C, Ultramid® T7300EG10 LS BK23346 (cond.), PA*-GF50, BASF
Módulo de fluência - tempo 23°C, Ultramid® T7300EG10 LS BK23346 (cond.), PA*-GF50, BASF
Curva de fluencia 23°C, Ultramid® T7300EG10 LS BK23346 (cond.), PA*-GF50, BASF
Tensão - deformação (isocrônico) 80°C, Ultramid® T7300EG10 LS BK23346 (dry), PA*-GF50, BASF
Módulo de fluência - tempo 80°C, Ultramid® T7300EG10 LS BK23346 (dry), PA*-GF50, BASF
Curva de fluencia 80°C, Ultramid® T7300EG10 LS BK23346 (dry), PA*-GF50, BASF
Módulo de tração - temperatura , Ultramid® T7300EG10 LS BK23346 (dry), PA*-GF50, BASF
Módulo de tração - temperatura , Ultramid® T7300EG10 LS BK23346 (cond.), PA*-GF50, BASF
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos, Negro
Características especiais
Estável contra o calor
Características
Impressora a laser
Aplicaciones
Automóvel, Elétrica e Eletrônica
Disponibilidade regional
Outras informações
Moldagem por injeção
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 110 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 280 - 310 °C
injection molding, Melt temperature, recommended: 300 °C
injection molding, Mold temperature, range: 80 - 120 °C
injection molding, Mold temperature, recommended: 100 °C
injection molding, Dwell time, thermoplastics: 5 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.